Stainless steel welded pipe requires deep weld penetration, no oxide inclusions, and the heat-affected zone as small as possible, tungsten inert gas shielded argon arc welding has better adaptability, high welding quality, good weld penetration performance, and its products in the chemical industry, the nuclear industry, and food and other industries are widely used.
Welding speed is not high is the shortcomings of argon arc welding, in order to improve the welding speed, foreign research and development of a variety of methods. Among them by a single electrode single torch development using multi-electrode multi-torch welding method in the production of applications. 70s Germany first used more than the torch along the weld direction straight-line arrangement, the formation of a long form of heat flow distribution, significantly improve the welding speed. General use of three electrode torch argon arc welding, welding steel pipe wall thickness S Greater than or equal to 2mm, welding speed than a single torch to improve 3-4 times, welding quality can also be improved. Argon arc welding and plasma welding can be combined to weld a larger wall thickness of steel pipe, in addition, in the argon gas 5-10 percent of hydrogen, and then using a high-frequency pulsed welding power supply can also improve the welding speed.
Multi-torch argon arc welding is suitable for austenitic and ferritic stainless steel pipe welding.
High-frequency welding
High-frequency welding for carbon steel welded pipe production has a history of more than 40 years, but for welding stainless steel pipe is a relatively new technology. The economy of its production is so that its products are more widely used in the field of architectural decoration, household appliances, and mechanical structures.
High-frequency welding has a higher power source power, for different materials, the OD wall thickness of the steel pipe can achieve a higher welding speed. Compared with argon arc welding, it is more than 10 times its maximum welding speed. Therefore, the production of general-purpose stainless steel pipe has a high productivity.
Because of the high-frequency welding speed, the removal of burrs in the welded pipe brings difficulties. At present, high-frequency welded stainless steel pipe is not yet acceptable for the chemical and nuclear industries, which is one of the reasons.
From the welding material, high-frequency welding can weld various types of austenitic stainless steel pipe. At the same time, the development of new steel grades and advances in molding welding methods, but also successfully welded ferritic stainless steel AISI409 and other steel grades.
A combination of welding methods is argon arc welding plus plasma welding, high-frequency welding plus plasma welding, high-frequency preheating plus three welding torch argon arc welding, and high-frequency preheating plus plasma plus argon arc welding. Combined welding to improve welding speed is very significant. For the use of high-frequency preheating of the combination of welded steel pipe weld quality and conventional argon arc welding, plasma welding is comparable to the welding operation is simple, the entire welding system is easy to automate, this combination is easy to interface with the existing high-frequency welding equipment, low investment costs, good benefits.

1. TIG welding has been widely used in production, it can obtain high-quality weld, commonly used to weld non-ferrous metals, stainless steel, ultra-high strength steel, and other materials. However, TIG welding has the disadvantages of shallow depth of fusion ( Less than or equal to 3mm), low welding efficiency, etc., for thick plates need to beveled for multi-pass welding. Increasing the welding current can make the depth of fusion increase, but the melt width and melt pool volume to increase the magnitude of the increase in the depth of fusion is much larger than the increase in the magnitude of the depth of fusion.
2. Activated TIG welding method has attracted worldwide attention in recent years. This technology is before welding the weld surface coated with a layer of active flux (referred to as an active agent), in the same welding specifications, compared with conventional TIG welding, which can significantly increase the depth of fusion (up to 300 percent ). For 8mm thick plate welding can not open the bevel once to obtain a greater depth of fusion or a weld penetration, for the thin plate can not change the welding speed in the case of reducing the welding heat input. At present, A-TIG welding can be used to weld stainless steel, carbon steel, nickel-based alloys and titanium alloys, and other materials. Compared with traditional TIG welding, A-TIG welding, can greatly improve productivity, and reduce production costs, but also can reduce welding deformation, which has very important application prospects. A-TIG welding key factor is the active agent composition selection. Currently, commonly used active agent components are mainly oxides, chlorides, and fluorides, different materials, and the applicable active agent composition is different. However, due to the importance of this technology, active agent compositions and formulations are patent-restricted at both PWI and EWI and are rarely reported in open publications. The current research on A-TIG welding mainly focuses on two aspects: the research on the mechanism of active agent action and the research on the application technology of activated welding.
3. There are three main types of active agents developed and used at home and abroad: oxides, fluorides, and chlorides. Early developed by PWI for titanium alloy welding active agent to oxides and chlorides, but the toxicity of chlorides is not conducive to the promotion and application. At present, foreign welding of stainless steel, carbon steel, and other active agents used an oxide-based, but the welding of titanium alloy materials contains a certain amount of active agent fluoride components.
4. Single component of the active agent on the stainless steel weld molding effects.
(1) For the weld coated with SiO2 active agent, with the increase in the amount of SiO2 coating, the width of the weld channel gradually becomes narrower, and the arc crater becomes longer, narrower, and deeper. The residual height at the back of the welding channel becomes higher, and at the intersection of coated active agent and uncoated active agent, the weld metal accumulates more, and among all the active agents, SiO2 has the greatest effect on weld shaping.
(2) The effect of active agent NaF and Cr2O3 on weld channel shaping is not obvious. With the increase in the amount of coating, the weld width did not change much, and the arc crater did not change significantly. Compared with the weld with no active agent, the weld bead width also did not change significantly, but the arc crater was larger than that of the inactive agent.
(3) With the increase of TiO2 coating amount, the appearance of the weld bead did not change much, and the arc crater did not change significantly, similar to that of the inactive flux. However, the surface of the weld formed is relatively flat and regular, and there is no biting phenomenon, which is better than the formation of the weld channel without an active agent.
(4) The active agent CaF2 has a greater effect on weld channel formation. With the increase in the amount of CaF2 coating, the weld bead formation becomes worse, the arc crater does not change much, and the weld width does not change much. However, with the increase in the amount of CaF2, there are defects such as biting edges.
(5) The effect on the melting depth, compared with the inactive agent, the above five active agents can increase the melting depth of the weld, and with the increase in the amount of coating, the depth of melting is also increased accordingly. However, when the amount of coating reaches a certain value, the depth of fusion increases to saturation and then increases the amount of coating, the depth of fusion instead of decreasing.